Additive manufacturing (AM) has gained increased significance and has been adopted across many industries for various applications. Specific net-shape AM fabrication methods, such as laser powder-bed fusion (LPBF), have matured significantly, leading to aerospace sector R&D focused on the feasibility of using flagship alloys to manufacture complex components. This article presents one example of an aluminum alloy design tailored for laser powder-bed fusion AM. It discusses the integrated computational materials engineering design approach. The article also presents the design for high-strength, high-temperature aluminum alloys.