Abstract
Additive manufacturing (AM) security is considered an integral part of several broader security fields, including supply chain security and critical infrastructure security. This article presents a general guide to the types of data and locations of data as they may exist in a typical AM-using organization. It discusses the following threat categories: technical data theft, sabotage, illegal part manufacturing, and data infiltration and exfiltration. The article also presents a detailed discussion on countermeasures against threat categories.
Mark Yampolskiy, Jacob Gatlin, Data Security in Additive Manufacturing, Additive Manufacturing Design and Applications, Vol 24A, ASM Handbook, Edited By Mohsen Seifi, David L. Bourell, William Frazier, Howard Kuhn, ASM International, 2023, p 203–209, https://doi.org/10.31399/asm.hb.v24A.a0006962
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.