Methodologies and Implementation of Laser Powder-Bed Fusion Process Control Available to Purchase
-
Published:2023
Abstract
Part quality in additive manufacturing (AM) is highly dependent on process control, but there is a lack of adequate AM control methods and standards. Laser powder-bed fusion (L-PBF) is one of the most-used metal AM techniques. This article focuses on the following laser control parameters: laser focus, laser power, laser position, and laser power-position synchronization. It then provides a discussion on laser scan strategies. The article also provides an overview of the AM control framework, the two major sections of which are software and hardware.
Ho Yeung, Methodologies and Implementation of Laser Powder-Bed Fusion Process Control, Additive Manufacturing Design and Applications, Vol 24A, ASM Handbook, Edited By Mohsen Seifi, David L. Bourell, William Frazier, Howard Kuhn, ASM International, 2023, p 388–396, https://doi.org/10.31399/asm.hb.v24A.a0006955
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.