Pneumatic Extrusion of Biomaterials
-
Published:2022
Abstract
This article focuses on the pneumatic extrusion-based system for biomaterials. It provides an overview of additive manufacturing (AM) processes, followed by sections covering steps and major approaches for the 3D bioprinting process. Then, the article discusses the types, processes, advantages, limitations, and applications of AM technology and extrusion-based approaches. Next, it provides information on the research on extrusion-based printing. Finally, the article provides a comparison of the extrusion-based approach with other approaches.
Sign in
ASM members
Member Sign InMahsius Sami, Prativa Das, Rahim Esfandyarpour, Pneumatic Extrusion of Biomaterials, Additive Manufacturing in Biomedical Applications, Vol 23A, ASM Handbook, Edited By Roger J. Narayan, ASM International, 2022, p 318–333, https://doi.org/10.31399/asm.hb.v23A.a0006893
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!