Laser-Induced Forward Transfer of Biomaterials
-
Published:2022
Abstract
The use of 3D bioprinting techniques has contributed to the development of novel cellular patterns and constructs in vitro, ex vivo, and even in vivo. There are three main bioprinting techniques: inkjet printing, extrusion printing (also known as bioextrusion), laser-induced forward transfer (LIFT) printing, which is also known as modified LIFT printing, matrix-assisted pulsed-laser evaporation direct write, and laser-based printing (laser-assisted bioprinting, or biological laser printing). This article provides an overview of the LIFT process, including the LIFT process introduction, different implementations, jetting dynamics, printability phase diagrams, and printing process simulations. Additionally, materials involved during LIFT are introduced in...
Sign in
ASM members
Member Sign InMarc Sole-Gras, Yong Huang, Douglas B. Chrisey, Laser-Induced Forward Transfer of Biomaterials, Additive Manufacturing in Biomedical Applications, Vol 23A, ASM Handbook, Edited By Roger J. Narayan, ASM International, 2022, p 252–265, https://doi.org/10.31399/asm.hb.v23A.a0006860
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!