Abstract
Discontinuities are interruptions in the desirable physical structure of a weld. This article describes the types of weld discontinuities that are characteristic of the principal welding processes. Discontinuities covered are metallurgical discontinuities, discontinuities associated with specialized welding processes, and base metal discontinuities. In addition, information on the common inspection methods used to detect these discontinuities is provided.
Topics
Microstructure,
Galvanic corrosion,
Intergranular corrosion,
Weld corrosion,
Deformation and fracture,
Fitness-for-service assessment,
Welding defects,
Cast iron,
Steel,
Cast nickel-based superalloys,
Wrought nickel-based superalloys,
Aluminum alloys,
Molybdenum alloys,
Nickel alloys,
Niobium alloys,
Tantalum alloys,
Titanium alloys,
Tungsten alloys,
Weldability testing,
Stress relieving,
Diffusion welding,
Explosion welding,
Arc welding,
Braze welding,
Butt welding,
Directed-energy fusion welding,
Resistance welding,
Alloy composition,
Weld strength,
Weldability,
Nondestructive testing,
Fracture toughness,
Ductility,
Shear strength,
Tensile properties,
Fatigue and fracture mechanics analysis,
Constitution diagrams,
Solidification,
Weld discontinuities,
Welding
You do not currently have access to this chapter.
Citation
Weld Discontinuities and Imperfections, Weld Integrity and Performance, Edited By Steve Lampman, ASM International, 1997, p 57–70, https://doi.org/10.31399/asm.tb.wip.t65930057
Download citation file:
Related Book Content
Overview of Weld Discontinuities
Welding, Brazing, and Soldering
Solidification of Metals and Alloys
Metals Handbook Desk Edition (2nd Edition)
Failure Analysis of Steel Welds
Failure Analysis of Heat Treated Steel Components
Defects Leading to Failure
Fatigue and Fracture Understanding the Basics
Glossary of Terms: Welding, Brazing, and Soldering
Welding, Brazing, and Soldering
Fracture Mechanics and Service Fitness of Welds
Weld Integrity and Performance
Welding
Stainless Steels for Design Engineers
Joining Titanium and Its Alloys
Titanium Physical Metallurgy, Processing, and Applications
Investigation of Fatigue-Induced Socket-Welded Joint Failures for Small-Bore Piping Used in Power Plants
ASM Failure Analysis Case Histories: Power Generating Equipment
Structural Steels and Steels for Pressure Vessels, Piping, and Boilers
Metallography of Steels Interpretation of Structure and the Effects of Processing