Abstract
This article describes the weldability tests that are used to evaluate the effects of welding on such properties and characteristics as base-metal and weld-metal cracking; base-metal and weld-metal ductility; weld penetration; and weld pool shape and fluid flow. It also describes several weldability tests for evaluating cracking susceptibility, classified as self-restraint or externally loaded tests. The article discusses the processes, advantages, and disadvantages of the weld pool shape tests, the weld penetration tests, and the Gleeble test.
Weldability Testing, Weld Integrity and Performance, Edited By Steve Lampman, ASM International, 1997, p 23–35, https://doi.org/10.31399/asm.tb.wip.t65930023