Tempering of Steels[1]
Revising author
Revising author
-
Published:2013
Abstract
Tempering of steel is a process in which hardened or normalized steel is heated to a temperature below the lower critical temperature and cooled at a suitable rate, primarily to increase ductility, toughness, and grain size of the matrix. This article provides an overview of the variables that affect the microstructure and mechanical properties of tempered steel, namely, the tempering temperature, tempering time, carbon content, alloy content, and residual elements. Tempering after hardening is performed to relieve quenching stresses and ensure dimensional stability of steel. The article discusses the embrittlement problems associated with tempering. Four types of equipment are used for tempering, namely, convection furnaces, salt bath furnaces, oil bath equipment and molten metal baths. Special procedures for tempering are briefly reviewed.
Renata Neves Penha, Lauralice C.F. Canale, Jan Vatavuk, Steven Lampman, Tempering of Steels, Steel Heat Treating Fundamentals and Processes, Vol 4A, ASM Handbook, Edited By Jon L. Dossett, George E. Totten, ASM International, 2013, p 327–351, https://doi.org/10.31399/asm.hb.v04a.a0005815
Download citation file:
Data Ecosystem
The ASM Data Ecosystem arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.