Steel Heat Treating Fundamentals and Processes
Flame Hardening of Steels[1]
Revising author
-
Published:2013
Abstract
Flame hardening is a heat treating process in which a thin surface shell of a steel part is heated rapidly to a temperature above the critical temperatures of the steel. The versatility of flame-hardening equipment and the wide range of heating conditions obtainable with gas burners, often permit flame hardening to be done by a variety of methods. These include the spot or stationary method, progressive method, spinning method, and the combination progressive-spinning method. This article provides information on fuel gases used in flame hardening and their selection criteria for specific applications. It also discusses operating procedures and control...
Sign in
ASM members
Member Sign InB. Rivolta, Flame Hardening of Steels, Steel Heat Treating Fundamentals and Processes, Vol 4A, ASM Handbook, Edited By Jon L. Dossett, George E. Totten, ASM International, 2013, p 419–437, https://doi.org/10.31399/asm.hb.v04a.a0005807
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!