Abstract
This article provides a detailed discussion on the factors involved in the selection of steels for austempering, including section thickness limitations of steel parts and modifications of austempering practice. The selection of steel for an austempered component is based on the processing characteristics of the heat treating equipment employed. It is also based on the hardenability and transformation characteristics of the steel alloy as indicated by time-temperature-transformation and isothermal-transformation diagrams. The article contains tables that compare the dimensional changes that occur in stabilizer bars as a result of oil quenching and tempering with those that resulted from austempering. It...
Sign in
ASM members
Member Sign InJohn R. Keough, Austempered Steel, Steel Heat Treating Fundamentals and Processes, Vol 4A, ASM Handbook, Edited By Jon L. Dossett, George E. Totten, ASM International, 2013, p 352–360, https://doi.org/10.31399/asm.hb.v04a.a0005810
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.