Austenitization refers to heating into the austenite phase field, during which the austenite structure is formed. This article highlights the purpose of austenitization, and reviews the mechanism and importance of thermodynamics and kinetics of austenite structure using an iron-carbon binary phase diagram. It also describes the effects of austenite grain size, and provides useful information on controlling the austenite grain size using the thermomechanical process.