Manufacturing-Related Failures of Plastic Parts Available to Purchase
-
Published:2022
Abstract
This article focuses on manufacturing-related failures of injection-molded plastic parts, although the concepts apply to all plastic manufacturing processes It provides detailed examples of failures due to improper material handling, drying, mixing of additives, and molecular packing and orientation. It also presents examples of failures stemming from material degradation improper use of metal inserts, weak weld lines, insufficient curing of thermosets, and inadequate mixing and impregnation in the case of thermoset composites.
Vishu Shah, Manufacturing-Related Failures of Plastic Parts, Characterization and Failure Analysis of Plastics, Vol 11B, ASM Handbook, Edited By Todd J. Menna, ASM International, 2022, p 599–609, https://doi.org/10.31399/asm.hb.v11B.a0006916
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.