Surface Examination and Analysis of Plastics
By
Sachin Attavar
Sachin Attavar
EAG Laboratories/Eurofins
Search for other works by this author on:
-
Published:2022
Abstract
This article discusses the operating principles, advantages, and limitations of scanning electron microscopy, atomic force microscopy, x-ray photoelectron spectroscopy, and secondary ion mass spectroscopy that are used to analyze the surface chemistry of plastics.
Topics
Chemical analysis,
Polymer degradation,
Polymers,
Polymer processing,
Chemical composition,
Engineering design,
Materials selection,
Root cause analysis,
Thermal analysis,
Plastics,
Scanning electron microscopy,
Atomic force microscopy,
Secondary ion mass spectrometry,
X-ray photoelectron spectroscopy,
Chemical analysis,
Polymer degradation,
Polymers,
Polymer processing,
Chemical composition,
Engineering design,
Materials selection,
Root cause analysis,
Thermal analysis
You do not currently have access to this chapter.
Citation
Sya Ensha, Paul West, Sachin Attavar, Surface Examination and Analysis of Plastics, Characterization and Failure Analysis of Plastics, Vol 11B, ASM Handbook, Edited By Todd J. Menna, ASM International, 2022, p 553–586, https://doi.org/10.31399/asm.hb.v11B.a0006943
Download citation file:
Related Book Content
Surface Analysis
Metals Handbook Desk Edition (2nd Edition)
Surface and Interface Analysis of Coatings and Thin Films
Surface Engineering
Surface Characterization for Medical Devices
Materials for Medical Devices
Secondary Ion Mass Spectroscopy
Materials Characterization (2019 Edition)
Wear Measurement
Friction, Lubrication, and Wear Technology
Applications of Modern Analytical Instruments in Corrosion
Corrosion: Fundamentals, Testing, and Protection
Metallographic Technique—Electron Microscopy and Other Advanced Techniques
Metallography of Steels Interpretation of Structure and the Effects of Processing
Atomic Force Microscopy
Materials Characterization (2019 Edition)
Secondary Ion Mass Spectroscopy
Materials Characterization
Plastic Design Methods
Characterization and Failure Analysis of Plastics