Weathering Testing of Polymeric Materials Available to Purchase
-
Published:2022
Abstract
This article presents a general overview of outdoor weather aging factors, their effects on the performance of polymeric materials, and the accelerated test methods that can be used to investigate those effects. These test methods are used to characterize material performance when subjected to specific, often controlled, and well-defined factors. The article also presents an overview of weathering instrument types that simulate outdoor stress factors.
Florian Feil, Matt McGreer, Weathering Testing of Polymeric Materials, Characterization and Failure Analysis of Plastics, Vol 11B, ASM Handbook, Edited By Todd J. Menna, ASM International, 2022, p 1–8, https://doi.org/10.31399/asm.hb.v11B.a0006871