The chapter presents an overview of the properties and operational limits of superconductive materials, as well as techniques used to fabricate practical superconducting wires. It introduces six properties: critical temperature, critical magnetic field, critical current density, stability, ac loss, and mechanical characteristics; for each property, typical data are provided and the experimental methods used to measure it are briefly described. The properties of the superconducting composites are tied together in the chapter to summarize their effect on superconductor material selection and the geometrical design of superconducting composites. The chapter also contains a reference guide to composite-design factors with links...