Abstract
This chapter discusses the structural alloys being used for cryogenic applications in commercially significant quantities. It emphasizes the practical considerations involved in the material selection process and provides the information necessary to make preliminary selections of alloys most suitable for the intended cryogenic application. The chapter provides general information on a class or group of alloys, their representative mechanical and physical properties, and their fabrication characteristics. The materials covered are austenitic stainless steels, nickel steels, aluminum alloys, and other metals and alloys.
Sign in
ASM members
Member Sign InH. I. McHenry, Structural Alloys, Materials at Low Temperatures, Edited By Richard P. Reed, Alan F. Clark, ASM International, 1983, p 371–411, https://doi.org/10.31399/asm.tb.mlt.t62860371
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!