Abstract
This chapter discusses the history of hardness testing and defines the term hardness. It describes the interrelationship between material structure and hardness and the relationships between hardness and other mechanical material properties. In addition, information on the hardness unit and traceability of the hardness measurement are provided.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
K. Herrmann, The Fundamentals of Hardness Testing, Hardness Testing: Principles and Applications, Edited By Konrad Herrmann, ASM International, 2011, p 1–23, https://doi.org/10.31399/asm.tb.htpa.t53310001
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!
Related Book Content
Hardness
Metallography Principles and Practice
Hardness and Hardenability
Practical Heat Treating (Second Edition)
Gage Repeatability and Reproducibility in Hardness Testing
Mechanical Testing and Evaluation
Inspection of Powder Metallurgy Parts
Inspection of Metals Understanding the Basics
Examination of the Nitrided Case
Practical Nitriding and Ferritic Nitrocarburizing
Standards and Inspection
Practical Induction Heat Treating (Second Edition)
Hardness Measurement of Plastics and Elastomers
Hardness Testing Principles and Applications
Introduction to Hardness Testing
Mechanical Testing and Evaluation
The Role of Elasticity in Hardness Testing
Mechanical Testing and Evaluation
Qualification Testing for Coating System Selection
Protective Organic Coatings