Handbook of Case Histories in Failure Analysis
Failure Analysis of NiTi Wires Used in Medical Applications
-
Published:2019
Abstract
Superelastic nitinol wires that fractured under various conditions were examined under a scanning electron microscope in order to characterize the fracture surfaces, produce reference data, and compare the findings with prior published work. The study revealed that nitinol fracture modes and morphologies are generally consistent with those of ductile metals, such as austenitic stainless steel, with one exception: Nitinol exhibits a unique damage mechanism under high bending strain, where damage occurs at the compression side of tight bends or kinks while the tensile side is unaffected. The damage begins as slip line formation due to plastic deformation, which progresses...
Sign in
ASM members
Member Sign InB. James, J. Foulds, L. Eiselstein, Failure Analysis of NiTi Wires Used in Medical Applications, Handbook of Case Histories in Failure Analysis, Vol 3, Edited By Larry Berardinis, ASM International, 2019, p 349–354, https://doi.org/10.31399/asm.fach.v03.c9001802
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!