In this article, we report the outcome of an investigation made to uncover the premature fracture of crusher jaws produced in a local foundry. A crusher jaw that had failed while in service was studied through metallographic techniques to determine the cause of the failure. Our investigation revealed that the reason for the fracture was the presence of large carbides at the grain boundaries and in the grain matrix. This led to the formation of microcracks that propagated along the grain boundaries under in-service working forces. It is also believed that the precipitation of carbides at the grain boundaries may have occurred because of improper heat treatment, but not because of a deficiency in composition.
J.O. Olawale, S.A. Ibitoye, M.D. Shittu, A.P.I. Popoola, A Study of Premature Failure of Crusher Jaws, Handbook of Case Histories in Failure Analysis, Vol 3, Edited By Larry Berardinis, ASM International, 2019, p 172–176, https://doi.org/10.31399/asm.fach.v03.c9001776
Download citation file:
New Handbook: Volume 11B
Now available in the Digital Library! Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.