During the installation of power transmission lines across a major interstate highway, a temporary anchor stabilizing one of the poles failed, resulting in the loss of the pole and the associated power lines. It also contributed to a single vehicle incident on the adjacent roadway. Post-failure analysis revealed that the fracture was precipitated by a preexisting weld-related crack. Closed form and numerical stress analyses were also conducted, with the results indicating that the anchor was installed properly within the parameters intended by the manufacturer.
Sign in
ASM members
Member Sign InM.E. Stevenson, M.E. Barkey, J.L. McDougall, E.R. Weishaupt, Failure Analysis of a Temporary Power Line Anchor, Handbook of Case Histories in Failure Analysis, Vol 3, Edited By Larry Berardinis, ASM International, 2019, p 101–106, https://doi.org/10.31399/asm.fach.v03.c9001766
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!