Handbook of Case Histories in Failure Analysis
Pitting Corrosion of Stainless Steel by Potable Municipal Water in an Organic Chemical Plant
-
Published:1992
Abstract
Several tubes in a 35 m2 (115 ft2) type 316 stainless steel shell-and-tube condenser leaked unexpectedly in an organic chemical plant that produces vinyl acetate monomer. Leaks were discovered after 5 years of operation and relocation of the condenser to another unit in the same plant. Examination of tubes and tube sheets revealed pitting damage on the OD surface. Some of the pits had penetrated fully, resulting in holes. Inside diameter surfaces were free of corrosion. Macro- and microexaminations indicated that the tubes had been properly manufactured. Pitting was attributed to stagnant water on the shell side. It was recommended that the surfaces not be kept in contacts with closed stagnant water for appreciable lengths of time.
K.E. Perumal, Pitting Corrosion of Stainless Steel by Potable Municipal Water in an Organic Chemical Plant, Handbook of Case Histories in Failure Analysis, Vol 1, Edited By Khlefa A. Esaklul, ASM International, 1992, p 176–177, https://doi.org/10.31399/asm.fach.v01.c9001063
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!