ASM Handbook
Properties and Selection: Irons, Steels, and High-Performance Alloys
ASM International
Volume
1
ISBN electronic:
978-1-62708-161-0
Publication date:
1990
Abstract
This article discusses the following physical properties of AISI and SAE grades of carbon and low-alloy steels: coefficients of linear thermal expansion; thermal conductivity; specific heat; and electrical resistivity.
This content is PDF only. Please click on the PDF icon to access.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Physical Properties of Carbon and Low-Alloy Steels, Properties and Selection: Irons, Steels, and High-Performance Alloys, Vol 1, ASM Handbook, By ASM Handbook Committee, ASM International, 1990, p 195–199, https://doi.org/10.31399/asm.hb.v01.a0001010
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Physical Properties of Carbon and Low-Alloy Steels
Failure Analysis of Heat Treated Steel Components
Classification and Designation of Carbon and Low-Alloy Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Flux Cored Arc Welding
Welding Fundamentals and Processes
Elevated-Temperature Properties of Ferritic Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Procedure Development and Practice Considerations for Ultrasonic Welding
Welding, Brazing, and Soldering
Fatigue Resistance of Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Hardenability of Carbon and Low-Alloy Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Service Characteristics of Carbon and Alloy Steels
Metals Handbook Desk Edition (2nd Edition)
Microstructures, Processing, and Properties of Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Procedure Development and Practice Considerations for Diffusion Welding
Welding, Brazing, and Soldering