Properties and Selection: Irons, Steels, and High-Performance Alloys
Ductile Iron
Revising author
Revising author
-
Published:1990
Abstract
This article discusses the compositions, properties, and typical applications for ductile irons that are defined by U.S. and international standards . It describes the various methods used to test and inspect the metallurgical control processes in ductile iron production. The article discusses the effect of composition, graphite shape, and section size on the properties of ductile iron. The article also describes the mechanical properties of ductile iron at elevated temperatures. The heat treatment of ductile iron castings produces a significant difference in mechanical properties from as-cast ductile iron. A ductile iron generally has higher hardenability than a eutectoid steel with comparable alloy content. The article also discusses the physical properties of ductile iron, including density, thermal conductivity, electrical conductivity, electrical resistivity, and magnetic properties. Ductile iron has been chosen in many instances on the basis of significantly lower machining costs, which resulted in lower overall cost of the part.
Lyle R. Jenkins, R.D. Forrest, Ductile Iron, Properties and Selection: Irons, Steels, and High-Performance Alloys, Vol 1, ASM Handbook, By ASM Handbook Committee, ASM International, 1990, p 33–55, https://doi.org/10.31399/asm.hb.v01.a0001003
Download citation file:
New Handbook: Volume 11B
Now available in the Digital Library! Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.