Skip to Main Content
Skip Nav Destination

This article discusses the composition, characteristics, and properties of the five groups of wrought stainless steels: martensitic stainless steels, ferritic stainless steels, austenitic stainless steels, duplex stainless steels, and precipitation-hardening stainless steels. The selection of stainless steels may be based on corrosion resistance, fabrication characteristics, availability, mechanical properties in specific temperature ranges and product cost. The fabrication characteristics of stainless steels include formability, forgeability, machinability, and weldability. The product forms of wrought stainless steels are plate, sheet, strip, foil, bar, wire, semifinished products, pipes, tubes, and tubing. The article describes tensile properties, elevated-temperature properties, subzero-temperature properties, physical properties, corrosion properties, and fatigue strength of stainless steels. It characterizes the experience of a few industrial sectors according to the corrosion problems most frequently encountered and suggests appropriate grade selections. Corrosion testing, surface finishing, mill finishes, and interim surface protection of stainless steels are also discussed.

You do not currently have access to this chapter.
Don't already have an account? Register

or Create an Account

Close Modal
Close Modal