Abstract
Stainless steels are widely used at elevated temperatures when carbon and low-alloy steels do not provide adequate corrosion resistance and/or sufficient strength at these temperatures. This article deals with the wrought stainless steels used for high temperature applications. It gives some typical compositions of wrought heat-resistant stainless steels, which are grouped into ferritic, martensitic, austenitic, and precipitation-hardening (PH) grades. Quenched and tempered martensitic stainless steels are essentially martensitic and harden when air cooled from the austenitizing temperature. These alloys offer good combinations of mechanical properties. The article focuses on mechanical property considerations and corrosion resistance considerations of stainless steels. The corrosion and oxidation resistance of wrought stainless steels is similar to that of cast stainless steels with comparable compositions.
Elevated-Temperature Properties of Stainless Steels, Properties and Selection: Irons, Steels, and High-Performance Alloys, Vol 1, ASM Handbook, By ASM Handbook Committee, ASM International, 1990, p 930–949, https://doi.org/10.31399/asm.hb.v01.a0001048
Download citation file:
New Handbook: Volume 11B
Now available in the Digital Library! Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.