Carbon steels have wider usage than any other metal because of their versatility and low cost. Required hardenability is the most important factor influencing a choice between carbon- and alloy steel. By increasing hardenability, alloying elements extend the potential for enhanced properties to the large sections required for many applications. Alloy steels are ordinarily quench hardened and tempered to the level of strength desired for the application. Distortion during heat treatment may occur with almost any hardenable carbon or alloy steel, although distortion is usually more severe for carbon grades than for alloy grades of equivalent carbon content. The...
Sign in
ASM members
Member Sign InHardenability of Carbon and Low-Alloy Steels, Properties and Selection: Irons, Steels, and High-Performance Alloys, Vol 1, ASM Handbook, By ASM Handbook Committee, ASM International, 1990
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.