Mechanical Properties: Key Topics in Materials Science and Engineering
Appendix: Materials Testing for Mechanical Properties—Problems and Solutions
-
Published:2021
Abstract
This appendix provides readers with worked solutions to 25 problems involving calculations associated with tensile testing and the determination of mechanical properties and variables. The problems deal with engineering factors and considerations such as stress and strain, loading force, sample lengthening, and machine stiffness, and with mechanical properties and parameters such as elastic modulus, Young’s modulus, strength coefficient, strain-hardening exponent, and modulus of resilience. They also cover a wide range of materials including various grades of aluminum and steel as well as iron, titanium, brass, and copper alloys.
Sign in
ASM members
Member Sign InMaterials Testing for Mechanical Properties—Problems and Solutions, Mechanical Properties: Key Topics in Materials Science and Engineering, By Robert Tuttle, ASM International, 2021, p 19–37, https://doi.org/10.31399/asm.tb.mpktmse.t56010019
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.