Composite Filament Winding
Chapter 6: Control of Filament Winding Parameters
Deceased. Published with the assistance of the author’s son, Douglas McLarty
-
Published:2011
Abstract
This chapter addresses the hardware requirements for filament winding, from elementary processing equipment to more advanced systems. The chapter describes the equipment, defines how it is best used, and presents real-life examples. It describes a helical horizontal filament winding machine system and a vertical winding machine. The chapter provides information on in-plane (polar) winders and several types of creels, namely stationary and no twist, rotating, braking, and combinations thereof. Comprehensive descriptions of mandrel designs used in filament winding are presented in text and illustration. The chapter also reviews process control of filament winding parameters, including for some specialized winding...
Sign in
ASM members
Member Sign InJ. Lowrie McLarty, Control of Filament Winding Parameters, Composite Filament Winding, Edited By S.T. Peters, ASM International, 2011, p 65–79, https://doi.org/10.31399/asm.tb.cfw.t52860065
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.