Composite Filament Winding
Chapter 2: Automated Filament Winding Systems
-
Published:2011
Abstract
This chapter reviews the development of filament winding systems and the automated processes used in state-of-the-art filament winding facilities. It first provides a description on the early stages of modern filament winding, followed by brief information on the advances of filament winding in the computer age. Then, the chapter discusses the requirements for filament winding in manufacturing oil and gas industry components and in high-volume production of sporting goods, propane tanks, and curing ovens. The chapter concludes with examples of the versatility of filament winding in producing complex parts.
Sign in
ASM members
Member Sign InJohn E. Green, Automated Filament Winding Systems, Composite Filament Winding, Edited By S.T. Peters, ASM International, 2011, p 7–18, https://doi.org/10.31399/asm.tb.cfw.t52860007
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.