Failures of Cranes and Lifting Equipment
-
Published:2021
Abstract
The types of metal components used in lifting equipment include gears, shafts, drums and sheaves, brakes, brake wheels, couplings, bearings, wheels, electrical switchgear, chains, wire rope, and hooks. This article primarily deals with many of these metal components of lifting equipment in three categories: cranes and bridges, attachments used for direct lifting, and built-in members of lifting equipment. It first reviews the mechanisms, origins, and investigation of failures. Then the article describes the materials used for lifting equipment, followed by a section explaining the failure analysis of wire ropes and the failure of wire ropes due to corrosion, a...
Sign in
ASM members
Member Sign InBurak Akyuz, Nicholas Steinhoff, Failures of Cranes and Lifting Equipment, Analysis and Prevention of Component and Equipment Failures, Vol 11A, ASM Handbook, Edited By Brett A. Miller, Roch J. Shipley, Ronald J. Parrington, Daniel P. Dennies, ASM International, 2021, p 415–434, https://doi.org/10.31399/asm.hb.v11A.a0006830
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.