Sheet Metal Forming: Processes and Applications
Chapter 4: Progressive and Transfer Die Forming
-
Published:2012
Abstract
This chapter presents two case studies; one demonstrating the use of finite-element analysis (FEA) in the design of a progressive die forming operation, the other explaining how software simulations helped engineers reduce thinning and eliminate cracking and deformation observed in clutch hubs formed using a three-step transfer die process. It also discusses the role of FEA and commercial software in the design of progressive dies.
Sign in
ASM members
Member Sign InParth Pathak, Ajay Yadav, Progressive and Transfer Die Forming, Sheet Metal Forming: Processes and Applications, Edited By Taylan Altan, A. Erman Tekkaya, ASM International, 2012, p 73–82, https://doi.org/10.31399/asm.tb.smfpa.t53500073
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!