Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Metallic Glasses
-
Published:1990
Abstract
Metallic glasses can be prepared by solidification of liquid alloys at cooling rates sufficient to suppress the nucleation and growth of competing crystalline phases. This article presents a historical survey of the study of metallic glasses and other amorphous metals and alloys. This includes a discussion of synthesis and processing methods, structure and morphology, and a description of the electronic, magnetic, thermodynamic, chemical, and mechanical properties of metallic glasses. In addition, the article describes the development of metallic glasses as materials for technical applications.
Sign in
ASM members
Member Sign InW.L. Johnson, Metallic Glasses, Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, Vol 2, ASM Handbook, By ASM Handbook Committee, ASM International, 1990, p 804–821, https://doi.org/10.31399/asm.hb.v02.a0001095
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.