Properties of Cast Aluminum Alloys Available to Purchase
Revising author
-
Published:1990
Abstract
This article is a compilation of property data for standard grades of cast aluminum alloys. Data are provided for mechanical, thermal, and electrical properties. The listing for each alloy includes commercial names, chemical compositions, applications, relevant specifications, fabrication characteristics, and mass characteristics.
A.L. Kearney, Properties of Cast Aluminum Alloys, Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, Vol 2, ASM Handbook, By ASM Handbook Committee, ASM International, 1990, p 152–177, https://doi.org/10.31399/asm.hb.v02.a0001062