Properties of Wrought Coppers and Copper Alloys
Revising author
-
Published:1990
Abstract
This article is a compilation of the property data for standard grades of wrought copper and copper alloys. Data are provided for mechanical, physical, thermal, electrical, optical, and magnetic properties. The list for each alloy includes its commercial names, chemical composition, relevant specifications and standards, fabrication characteristics, mass characteristics, and applications.
Peter Robinson, Properties of Wrought Coppers and Copper Alloys, Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, Vol 2, ASM Handbook, By ASM Handbook Committee, ASM International, 1990, p 265–345, https://doi.org/10.31399/asm.hb.v02.a0001067