Ordered Intermetallics
-
Published:1990
Abstract
Ordered intermetallic compounds based on aluminides and silicides constitute a unique class of metallic materials that have promising physical and mechanical properties for structural applications at elevated temperatures. This article provides useful information on mechanical and metallurgical properties, material processing and fabrication, structural applications, mechanical behavior, environmental embrittlement, alloying effects, and crystal structure of aluminides of nickel, iron, titanium, and silicides. It describes the cleavage and intergranular fracture in trialuminides.
Sign in
ASM members
Member Sign InC.T. Liu, J.O. Stiegler, F.H. (Sam) Froes, Ordered Intermetallics, Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, Vol 2, ASM Handbook, By ASM Handbook Committee, ASM International, 1990, p 913–942, https://doi.org/10.31399/asm.hb.v02.a0001102
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!