This article focuses on different thin-film deposition techniques used to make superconducting films and discusses the properties and advantages of high-critical-temperature and low-critical-temperature materials in a number of applications, including signal processing and analog electronic devices. The article gives a brief introduction on superconducting materials, substrates and buffer layers and discusses the major deposition techniques such as, electron-beam co-evaporation, sputtering from either a composite target or multiple sources and laser ablation. The article also describes the in-situ film growth techniques for producing atomic oxygen by radio frequency excitation or microwave discharge or with ozone.