Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Uranium and Uranium Alloys
-
Published:1990
Abstract
Uranium is a moderately strong and ductile metal that can be cast, formed, and welded by a variety of standard methods. This article presents an overview of the processing and properties of uranium and uranium alloys with a brief overview of the principal hazards and precautions associated with processing depleted uranium and methods to control mild radioactivity, chemical toxicity, and pyrophoricity. It also describes the classification and heat treatment of uranium and uranium alloys. Furthermore, the article provides graphical representation of the effect of alloy composition, cooling rate, and aging temperature on microstructure, crystal structure, and mechanical properties of...
Sign in
ASM members
Member Sign InK.H. Eckelmeyer, Uranium and Uranium Alloys, Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, Vol 2, ASM Handbook, By ASM Handbook Committee, ASM International, 1990, p 670–682, https://doi.org/10.31399/asm.hb.v02.a0001085
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.