Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Titanium Powder Metallurgy Products
-
Published:1990
Abstract
This article focuses on the mechanical properties, production of titanium powder metallurgy (P/M) compacts, namely, blended elemental (BE) compacts and prealloyed (PA) compacts. It explains the postcompaction treatments of titanium P/M compacts, including heat treatment, and thermochemical processing. The article talks about the applications of titanium P/M products, namely, BE and PA products. It concludes with a short note on the future trends in titanium P/M technology.
Sign in
ASM members
Member Sign InDaniel Eylon, F.H. (Sam) Froes, Titanium Powder Metallurgy Products, Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, Vol 2, ASM Handbook, By ASM Handbook Committee, ASM International, 1990, p 647–660, https://doi.org/10.31399/asm.hb.v02.a0001083
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.