Properties of Precious Metals
-
Published:1990
Page range:
699 - 719
Abstract
This article discusses the chemical composition, fabrication characteristics, applications, mechanical properties, mass characteristics, thermal properties, electrical properties, optical properties, and chemical properties of precious metals, namely, silver, gold, platinum, and palladium and their corresponding alloys.
You do not currently have access to this chapter.
Citation
Properties of Precious Metals, Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, Vol 2, ASM Handbook, By ASM Handbook Committee, ASM International, 1990, p 699–719, https://doi.org/10.31399/asm.hb.v02.a0001088
Download citation file:
Bi-Weekly Supplement to AM&P Print Magazine
AM&P eNews delivers timely industry news, technology updates, fun videos and facts, and much more to materials professionals from around the globe.
Related Book Content
Properties of Cast Copper Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Properties of Pure Metals
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Properties of Wrought Coppers and Copper Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Engineering Plastics—An Introduction
Characterization and Failure Analysis of Plastics
Design and Engineering Properties of Glasses
Engineered Materials Handbook Desk Edition
Properties of Wrought Aluminum and Aluminum Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Properties of Cast Aluminum Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Effects of Composition, Processing, and Structure on Properties of Engineering Plastics
Materials Selection and Design
Properties of Magnesium Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Physical Properties of Metals
Elements of Metallurgy and Engineering Alloys