Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Tin and Tin Alloys
Revising author
-
Published:1990
Abstract
Tin is produced from both primary and secondary sources. This article discusses the chemical compositions, production, properties, microstructure and applications of tin and tin alloys. The major tin alloys discussed here are tin-antimony-copper alloy (pewter), bearing alloy, solder alloy and other alloys containing traces of tin. Data on tin consumption in the United States is presented graphically.
Sign in
ASM members
Member Sign InWilliam B. Hampshire, Tin and Tin Alloys, Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, Vol 2, ASM Handbook, By ASM Handbook Committee, ASM International, 1990, p 517–526, https://doi.org/10.31399/asm.hb.v02.a0001076