Failure Analysis and Prevention (2021 Edition)
Abstract
Corrosive wear is defined as surface damage caused by wear in a corrosive environment, involving combined attacks from wear and corrosion. This article begins with a discussion on several typical forms of corrosive wear encountered in industry, followed by a discussion on mechanisms for corrosive wear. Next, the article explains testing methods and characterization of corrosive wear. Various factors that influence corrosive wear are then covered. The article concludes with general guidelines for material selection against corrosive wear.
D.Y. Li, Corrosive Wear Failures, Failure Analysis and Prevention, Vol 11, 2021 ed., ASM Handbook, Edited By Brett A. Miller, Roch J. Shipley, Ronald J. Parrington, Daniel P. Dennies, ASM International, 2021, p 745–754, https://doi.org/10.31399/asm.hb.v11.a0006794
Download citation file:
New Handbook: Volume 11B
Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.