Sheet Metal Forming: Fundamentals
Chapter 12: Hydraulic Presses
-
Published:2012
Abstract
This chapter discusses the design and operation of hydraulic presses. It begins by describing the role of each major component in a hydraulic system. It then explains the difference between pump-driven and accumulator-driven presses and the types of applications for which are suited. The chapter goes on to describe the load, energy, and time-dependent characteristics of hydraulic presses and the factors that determine accuracy. It also explains how hydraulic presses are used for deep drawing, fine blanking, and hydroforming as well as warm forming and hot stamping operations.
Eren Billur, Hydraulic Presses, Sheet Metal Forming: Fundamentals, Edited By Taylan Altan, A. Erman Tekkaya, ASM International, 2012, p 181–201, https://doi.org/10.31399/asm.tb.smff.t53400181
Download citation file:
New Handbook: Volume 11B
Now available in the Digital Library! Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.