Book Chapter
Chapter 6: Materials for Sheet Forming
By
Soumya Subramonian
;
Soumya Subramonian
The Ohio State University
Search for other works by this author on:
Nimet Kardes
Nimet Kardes
The Ohio State University
Search for other works by this author on:
-
Published:2012
Abstract
This chapter describes the formability and forming characteristics of low-carbon sheet steels, coated sheet steels, stainless steels, and aluminum and magnesium alloys. It provides property data as well as flow stress curves for numerous grades of each material and explains how composition, microstructure, and processing methods influence forming behaviors.
Topics
Martensitic sheet steel,
Automotive sheet steels,
Sheet-metal forming dies,
Metal forming lubricants,
Drawing,
Bulk forming,
Sheet forming,
Process modeling and simulation,
Formability,
Deformation modeling,
Plastic deformation properties,
Low-carbon steel,
Stainless steel,
Aluminum alloys,
Magnesium alloys,
Flow stress
You do not currently have access to this chapter.
Citation
Soumya Subramonian, Nimet Kardes, Materials for Sheet Forming, Sheet Metal Forming: Fundamentals, Edited By Taylan Altan, A. Erman Tekkaya, ASM International, 2012, p 73–88, https://doi.org/10.31399/asm.tb.smff.t53400073
Download citation file:
Related Book Content
Plastic Deformation: Flow Stress, Anisotropy, and Formability
Sheet Metal Forming Fundamentals
Warm Forming of Magnesium and Aluminum Alloys
Sheet Metal Forming Processes and Applications
CAD/CAM and Die Face Design in Sheet Metal Forming
Metalworking: Sheet Forming
Forming of Aluminum Alloys
Aluminum Science and Technology
Forming
Stainless Steels for Design Engineers
Evaluating Intergranular Corrosion
Corrosion: Fundamentals, Testing, and Protection
Measurement and Interpretation of Flow Stress Data for the Simulation of Metal-Forming Processes
Metals Process Simulation
Procedure Development and Practice Considerations for Resistance Welding
Welding Fundamentals and Processes
Drop Hammer Forming
Metalworking: Sheet Forming
Heat Treatment of Nonferrous Alloys
Metallurgy for the Non-Metallurgist (Second Edition)