Coating Failures and Defects Available to Purchase
-
Published:2015
Abstract
Coatings, such as those applied to ships, must be resistant to abrasion, in the case of cargo hold coatings, and cyclic changes of chemicals and tank cleaning, in the case of tank linings. Failures and defects can manifest themselves at various times in the life of a coating. To determine the cause and mechanism of coating failure, all possible contributory factors must be evaluated together with a detailed history from the time of application to the time the failure was first noted. Many coating failures require further evaluation and analysis to be carried out by a qualified chemist or coating specialist, often using specialized laboratory equipment. The article presents examples of coating failures and defects, together with descriptions, probable causes, and suggested preventative measures.
Brendan Fitzsimons, Trevor Parry, Coating Failures and Defects, Protective Organic Coatings, Vol 5B, ASM Handbook, Edited By Kenneth B. Tator, ASM International, 2015, p 502–512, https://doi.org/10.31399/asm.hb.v05b.a0006008
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.