Alkyd Resins Available to Purchase
-
Published:2015
Abstract
An alkyd is an ester-based polymer derived from the polycondensation reaction of polyhydric alcohol and polybasic acid. This article provides useful information on the chemistry, production, coating formulations, modification, commercial products, and application methods of alkyd resins. It also provides a section on drying oil, which is used in the manufacture of resins. The article describes the three categories of metals that have been used in drier compounds: primary driers (active or oxidation driers), secondary driers (through-driers), and auxiliary driers. It also provides information on the oil length of an alkyd resin and on solvents, which play a critical role in the formulation and use of the coating. The article concludes with a description of the concerns that a user, specifier, or applicator should be aware of when using alkyd coatings.
Kenneth B. Tator, Michael G. Koehler, Alkyd Resins, Protective Organic Coatings, Vol 5B, ASM Handbook, Edited By Kenneth B. Tator, ASM International, 2015, p 39–47, https://doi.org/10.31399/asm.hb.v05b.a0006071
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.