Overview of Other Protection Methods[1] Available to Purchase
-
Published:2015
Abstract
This article provides a brief discussion on the common types of overlayers that can be used on a metal surface to protect it from corrosion. These overlayers include phosphate, chromate, and chromate-free conversion coatings; hot dip galvanizing; cementitious linings; glass and porcelain enamels; electroplating; thermal spray coatings; and rubber linings.
Kenneth B. Tator, Overview of Other Protection Methods, Protective Organic Coatings, Vol 5B, ASM Handbook, Edited By Kenneth B. Tator, ASM International, 2015, p 513–516, https://doi.org/10.31399/asm.hb.v05b.a0006027