Wax-Based Coating Systems Available to Purchase
-
Published:2015
Abstract
This article describes the features, benefits and limitations of petrolatum and microcrystalline wax. It provides a detailed discussion on the steps to be followed before applying the various forms of the wax-based coatings. The wax-based coating forms include petrolatum and microcrystalline tapes, marine petrolatum-based pile systems; cold-applied petrolatum-based paste coating systems; hot-applied microcrystalline wax flood coating systems; wax-based dips, brushons, and sprays; and wax-impregnated fabrics and wax-coated papers. The article also discusses the applications and limitations of these wax-based coatings. It concludes by highlighting the steps involved in the installation of wax-based casing fillers.
Charles Kennedy, Frank Rampton, Wax-Based Coating Systems, Protective Organic Coatings, Vol 5B, ASM Handbook, Edited By Kenneth B. Tator, ASM International, 2015, p 205–212, https://doi.org/10.31399/asm.hb.v05b.a0006048
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.