Fluoroethylene Vinyl Ether Resins for High-Performance Coatings Available to Purchase
-
Published:2015
Abstract
This article provides background information on the chemistry, coating properties, resin types, applications techniques, and performance characteristics of fluoroethylene vinyl ether (FEVE) resins. It describes the formulation methods of FEVE resins, namely, solvent-based coating formulations, water-based coating formulations, and powder coating formulations. The basic concerns to be addressed when formulating and using FEVE coatings are also discussed. The article concludes with a section on health and related safety regulations.
Robert Parker, Kristen Blankenship, Fluoroethylene Vinyl Ether Resins for High-Performance Coatings, Protective Organic Coatings, Vol 5B, ASM Handbook, Edited By Kenneth B. Tator, ASM International, 2015, p 88–95, https://doi.org/10.31399/asm.hb.v05b.a0006041
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.