Polyaspartic coating technology has found utility in a variety of coating applications, including corrosion protection and flooring topcoats, as these coatings are based on aliphatic polyisocyanates and aliphatic diamines. This article describes the chemistry of polyaspartic esters and curing characteristics and performance properties of polyaspartic coatings. It also provides information on curing corrosion protection coating systems, polyaspartic floor coatings, and safe-use recommendations for handling isocyanates.
Sign in
ASM members
Member Sign InEdward P. Squiller, Steven Reinstadtler, Polyaspartic Coatings, Protective Organic Coatings, Vol 5B, ASM Handbook, Edited By Kenneth B. Tator, ASM International, 2015, p 132–138, https://doi.org/10.31399/asm.hb.v05b.a0006036
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.