Polysiloxane Hybrid Coatings
-
Published:2015
Abstract
This article focuses on technologies in the protective coatings field, namely, polysiloxane hybrids and related materials. Industrial maintenance topcoats, including silicone alkyds, silicone epoxies, and polysiloxanes are reviewed. The article discusses two major application areas of protective coatings, namely, architectural coatings and automotive clear coats.
Gerald L. Witucki, Polysiloxane Hybrid Coatings, Protective Organic Coatings, Vol 5B, ASM Handbook, Edited By Kenneth B. Tator, ASM International, 2015, p 185–188, https://doi.org/10.31399/asm.hb.v05b.a0006029